Grade | Standard | Tensile strength Rm N/mm2 |
Yield strength ReL N/mm2 |
Light skin pass |
DC 01 | EN 10139 | 270 – 410 | ≤ 280 | LC |
DC 03 | EN 10139 | 270 – 370 | ≤ 240 | LC |
DC 04 | EN 10139 | 270 – 350 | ≤ 210 | LC |
Grade | Standard | Tensile strength Rm N/mm2 |
Yield strength ReL N/mm2 |
Light skin pass |
DC 01 | EN 10139 | 270 – 410 | ≤ 280 | LC |
DC 03 | EN 10139 | 270 – 370 | ≤ 240 | LC |
DC 04 | EN 10139 | 270 – 350 | ≤ 210 | LC |