Grade | Standard | Tensile strength Rm N/mm2 | Yield strength ReH N/mm2 mind. | Elongation at break A80% | Light skin pass |
C 22 E | EN 10132-3 | ≤ 500 | ≤ 400 | ≥ 22 | LC |
C 35 E | EN 10132-3 | ≤ 540 | ≤ 430 | ≥ 19 | LC |
C 40 E | EN 10132-3 | ≤ 550 | ≤ 440 | ≥ 18 | LC |
C 45 E | EN 10132-3 | ≤ 570 | ≤ 455 | ≥ 18 | LC |
C 55 E | EN 10132-3 | ≤ 600 | ≤ 480 | ≥ 17 | LC |
C 60 E | EN 10132-3 | ≤ 620 | ≤ 495 | ≥ 17 | LC |
25CrMo4 | EN 10132-3 | ≤ 580 | ≤ 440 | ≥ 19 | LC |
42CrMo4 | EN 10132-3 | ≤ 620 | ≤ 480 | ≥ 15 | LC |